I'd like to get my P3AT nickle or hard chrome plated - all parts that can be done. Note that there's people on the forum and also many others who offer this service. Do not want to do exchange with Kel Tec because I've got my gun working great and don't want to give up my "spiffed up" components. Am wondering if I just get my components plated if the added thickness of the plating will cause bind-up of slide, firing pin, extractor, etc. Does anyone have any experience with getting their guns plated that could give me a warm fuzzy that I would not screw things up with the action of my gun by doing this?
 

·
Registered
Joined
·
76 Posts
Discussion Starter · #3 ·
Thanks for input regarding plating yzguy. Good to hear that it won't change action of the gun. Some people indicate that the plating can even "slick up" the action. Will definitely consider going to Jack Fuselier if I do this based on many positive notes on his work.
 